Red : WT20, thorium content 1.7-2.2%, suitable for high current welding.
purple : WT30, thorium content is 2.8-3.2%, suitable for high current welding.
Brown : WZ3, zirconium content is 0.15-0.50%, suitable for AC current welding of aluminum alloy.
White : WZ8, zirconium content 0.70-0.90%, suitable for DC current welding under certain conditions.
Golden : WL15, lanthanum oxide content is 1.40-1.60%, suitable for welding a variety of alloys.
Dark blue : WL20, lanthanum oxide content is 1.80-2.20%, suitable for welding of a variety of alloys.
Gray : WC20, cerium oxide content 1.80-2.20%, suitable for low and medium current range welding.
gray : WR2, rare earth oxide mixture, cyan green, suitable for low and medium current range welding.
Wp-tungsten electrode:
Used for AC current welding of aluminum alloy
Not suitable for DC current welding
Wt-tungsten electrode:
The additive contains thorium, so there is a slight radiation
Because of the increased risk to health, so try not to use
It has better arc starting performance and higher current carrying capacity than pure tungsten electrode
The additive zirconium reduces the possibility of contamination of molten metal
Used for AC current welding of aluminum alloy
Only suitable for DC current welding under certain conditions
Wl-tungsten electrode:
Lanthanum oxide is beneficial to improve arc initiation performance
Suitable for both DC current welding and AC current welding
It can be used for welding non-alloy steel and high alloy steel, aluminum alloy, titanium alloy, nickel alloy, copper alloy and magnesium alloy, as well as for micro-beam plasma welding
Especially suitable for small current welding
Can be used to replace WT-tungsten electrode
Tungsten electrode containing cerium oxide has good arc initiation and re-initiation performance
Suitable for both DC current welding and AC current welding
It can be used to weld non-alloy and high-alloy steels, aluminum alloys, titanium alloys, nickel alloys, copper alloys and magnesium alloys in the low and medium current ranges
Can be used to replace WT-tungsten electrode
Ws-tungsten electrode:
There are different ingredients of additives, there is no uniform standard
Suitable for both DC current welding and AC current welding
It can be used to weld non-alloy and high-alloy steels, aluminum alloys, titanium alloys, nickel alloys, copper alloys and magnesium alloys in the low and medium current ranges
Long working life, high current carrying capacity
Amanda
Company: Baoji Dynamic Trading Co., Ltd
Country:China
Add:Baoti road,Jintai,Baoji city,Shaanxi,China
Cel/Whatsapp :+86 18309262795
Email:annie@jmyunti.com
Website:www.jm-titanium.com