Inner defect
1. Internal scarring
Features: The inner surface of the titanium tube shows scars, which generally do not take root and are easy to peel off.
Cause of occurrence:
1) Graphite lubricant contains impurities.
2) The iron ear at the back of the bare tube is pressed into the inner wall of the titanium tube, etc.
Inspection and judgment: The inner surface of the titanium tube is not allowed to exist, and the end of the tube should be polished and re cut. The grinding depth should not exceed the negative deviation required by the standard, and the actual wall thickness should not be less than the Z-value required by the standard; Scar formation within the entire length is considered invalid.
2. Inward folding
Features: Sawtooth shaped defects appear on the inner surface of the titanium tube in a straight or spiral or semi spiral shape.
Cause of occurrence:
1) Titanium billet: central porosity and segregation; Severe residual shrinkage; Non metallic inclusions exceeding the standard.
2) Uneven heating of the billet, high or low temperature, and prolonged heating time.
3) Perforated area: Severe wear on the top; Improper adjustment of perforating machine parameters; Aging of perforating rollers, etc.
Inspection and judgment: Internal bending is not allowed on the inner surface of the titanium tube. The internal bending at the end of the tube should be ground or re cut, and the actual wall thickness at the ground area should not be less than the standard requirement of Z small value; Full length internal folding is considered invalid.